Selection of flotation agents for tin ore

There are more than ten kinds of tin- containing minerals. At present, the tin used in industry is mainly derived from cassiterite. Due to the high density of cassiterite (6.4~7.1g/cm3), the main beneficiation method of cassiterite is re-election. However, due to the brittleness of the cassiterite, it is easy to mud in the natural world and in the process of crushing, grinding and sorting. Therefore, it is of great significance to recover the fine cassiterite from the re-election of fine mud and tailings by flotation.

A method of flotation of cassiterite is easy to be captured by various fatty acids and their soaps. Therefore, oleic acid, tal oil, oxidized paraffin soap, nylon 1010 lower foot, alkyl sulfate, alkyl sulfonate, sulfosuccinamide, etc., can be used as a collector of cassiterite. Experimental studies have shown that the use of toluic acid, benzyl phthalic acid and styrene phosphonic acid flotation of cassiterite can sometimes give better indicators.

When oleic acid is used as a collector to float the cassiterite, the pH is generally around 9.0 to 9.5. When toluene is used as a collector to float the cassiterite, the pH value of the rough selection is generally 5-6, and the selected pH value can be reduced to 2.5~4.0. When adjusting the pH value of the slurry, chemicals such as sodium hydroxide, sodium carbonate and sulfuric acid are often used. Cassiterite flotation, the suppression is useful to add water glass silicate minerals associated with hexametaphosphate, sodium phosphate, magnesium, calcium carboxymethylcellulose inhibiting mineral, wolframite added oxalic suppressed.

The raw material for flotation is generally a re-selected tailings of less than 0.04 mm, and the slime less than 0.01 mm is first removed. If the pulse is tin ore flotation, often associated sulfide minerals of iron, arsenic, antimony, lead, copper, zinc and other metals. At this time, the sulfide mineral is first floated out with the activator of the sulfide mineral, and then the cassiterite is floated to prevent the sulfide from contaminating the cassiterite concentrate.

B-Silver Flotation Example The ore of a tin mine is a high- and medium-temperature hot-liquid cassiterite deposit. Complex mineral composition, pyrite metal magnetic minerals, magnetite, pyrite, arsenopyrite, bismuthinite, galena, sphalerite and chalcopyrite, non-metallic mineral carbonates, silicates Salts and halides. The cassiterite is yellow-brown and black, with fine-grained inlays. Most of the powdered aggregates are embedded in the pyrrhotite, and a small part is scattered in the magnetite and skarn minerals. The largest grain is 0.55mm, the smallest is 0.002mm, and is generally between 0.15~0.02mm. The ore supply of cassiterite flotation is tailings after desulfurization, de-ironing and shaker recovery of coarse-grained cassiterite.

The shaker tailings advanced dehumidifier is dehydrated, and after dehydration, the tailings are discarded by the centrifuge. The centrifuge concentrate is dehydrated by a thickener and then added to the agitation tank for dosing and mixing. Salicylic acid is used as a collector, sodium carbonate is adjusted to pH value of 7~8, tannin is used as inhibitor, and No. 2 oil is used as foaming agent. The tin concentrate is selected after a coarse, two sweep, three fine and one fine sweep. The ore contains 1.0%~1.3% tin, the flotation concentrate grade is 1.3%~16%, and the recovery rate is 72%~76%.

Production practice shows that the low-toxic salicylic acid can completely replace the highly toxic tannic acid, which greatly reduces the environmental pollution problem in the production and use of pharmaceuticals. Tin mud, tin smelting slag beneficiation agent (national patent: code ZN801) Brand: Zhongnan tin-selecting agent Use purpose: tin mud, smelting slag, tin-flotation performance: good harvesting and selectivity, can replace traditional Benzene The choice of tin based on acid is overcome by the disadvantages of expensive and toxic benzyl phthalic acid agents.

Recommended dosage: 400-800 g / ton ore preparation method: 2-5% aqueous solution (weight ratio), dissolved in 40 ° C warm water. Scope of application: low-grade tin mud, smelting slag, 1.5% tin can be selected to more than 40% tin concentrate powder at room temperature (minimum temperature 5 ° C), the recovery rate is more than 70%. Environmental performance: low toxicity, friendly to humans and environment, easy to biodegrade.

Features: 1. Properties: The product is pink to orange-red paste to powdery solid, slightly soluble in water, soluble in alkaline solution, stable in nature. 2. Efficiently select new tin chemicals for the national 973 project; 3. The drug system is simple and low cost; 4. Environmentally friendly. The ZN801-collector has good selectivity under certain conditions. The product can form stable chelates with metals such as tin, tungsten, rare earth, copper, iron, etc., and forms unstable chelates with alkaline earth metals and alkali metals. Therefore, ZN-801 is flotation in certain metal minerals. The job shows a good sorting effect.

Corrosion-resistant fluorine gold mica gaskets dozens of varieties, more than 1,000 kinds of specifications, Changchun Taiyuan Fluorine Gold Mica Co., Ltd. produces Corrosion-Resistant Gasket materials, manufacturers real materials, welcome site visits. Corrosion-resistant fluorine gold mica gasket in the end Well there, samples are provided free of charge. Changchun Taiyuan Mica Film Production Base is looking forward to your visit. Can corrosion-resistant gasket materials save money?

Corrosion Resistant Mica Gasket

Corrosion Resistant Mica Gasket,Corrosion Resistant Materials,Corrosion-Resistant Gasket,Corrosion Resistance Corrugated Composite Gasket

Changchun City Taiyuan FluorphlogopiteCo. Ltd. , https://www.micaslice.com